Tag: nanoindenting
-
Creating deterministically placed single photon emitters in hexagonal boron nitride
Richarda NiemannVanderbilt University, Nashville, Tennessee, USA _______________________________________ With the rapidly increasing interest in quantum information technologies the miniaturization of on-chip devices using quantum photonic circuits has become a critical field of research. A central building block for these circuits are single photon emitters (SPEs) [1]. It was shown that a variety of materials can host…